Skip to main content
. 2020 Nov 10;12(11):2638. doi: 10.3390/polym12112638

Figure 6.

Figure 6

AFM images of PNIPAm b films spin-coated on glass-OH, glass-TMSPMA and glass-TMOS at 5000 rpm from a dispersion of 3 wt%, after being washed in water at 20 °C.