. 2020 Nov 19;13(22):5226. doi: 10.3390/ma13225226

Figure 16.

Figure 16

SEM images of fatigue surfaces of a specimen tested at a strain amplitude of 0.35%: (a) overall view of the fracture surface, (b) magnified view of the crack initiation zone, and (c) propagation region near the initiation site. The yellow arrows indicate the secondary cracks.