Figure 18.

Figure 18

SEM images of fatigue surfaces of a specimen tested at a strain amplitude of 0.8%: (a) overall view of the fracture surface, (b) upper part of the SZ surface, and (c) magnified view of the SZ surface. The yellow arrows indicate the secondary cracks.