Figure 4.

Figure 4

The signal charge spectrum evolution for the scCVD diamond sample irradiated with 200 MeV pions biased at E = +2 V/μm. The pulse height spectrum before irradiation was measured using a setup with a 90Sr β-source and a single pad metallization on the diamond, biased at 1 V/μm, since the detector collects all the charge at a bias voltage of 200 V. The integral of each spectrum was normalized to unity.