Figure 6.

Figure 6

The 1/λ for pCVD diamond in the fast neutron irradiation. The two values shown at each fluence are the values for positive (solid markers) and negative (open markers) bias at E= ±2 V/μm. The data were fit with a first-order damage curve independently for each sample.