Skip to main content
. 2020 Nov 27;11:1789–1800. doi: 10.3762/bjnano.11.161

Figure 4.

Figure 4

Pillars deposited at 38 pA. a) 35° tilt image of pillars deposited from top to bottom and from left to right from Pt(CO)2Cl2. b) 35° tilt image of pillars from MeCpPtMe3, rotated for better visibility. Scale bars are 500 nm.