Groups Flexural Strength (MPa) *** Elastic Modulus (MPa) * Modulus of Resilience (MPa) *** Vickers Microhardness (kg/mm2) ***
Control 86.35 ± 6.78 a 2640.00 ± 50.25 a 1.41 ± 0.19 a 14.98 ± 0.52 a
ND 101.76 ± 7.44 b 2735.08 ± 158.70 ab 1.88 ± 0.17 b 17.96 ± 1.07 c
A-ND 111.21 ± 7.43 b 2816.25 ± 73.83 b 2.20 ± 0.25 c 16.98 ± 0.62 b

Same lowercase letters indicate no significant differences in vertical column. * p ≤ 0.05, *** p ≤ 0.001 for comparison between the groups.