Fig. 7.

Fig. 7

A. Representative micro-CT images acquired at 4, 8 and 12 weeks: New bone formation of ulna and the morphology of the tubes after degradation. B. the corrosion rate (CR) of different coated Mg–Sr devices were calculated at 4, 8 and 12 weeks after implantation (**p˂0.01).