Elastic modulus of three different polyacrylamide gels assessed by AFM and compared to those obtained by AFM in Elosegui-Alberto et al. (2014) for the same formulations

Acr 5.5%/Bis 0.03% Acr 7.52%/Bis 0.16% Acr 12.0%/Bis 0.15%
Number of data 300 300 300
Maximum value (Emax) (kPa) 3.41 23.01 37.34
Mean value (Em) ± SD (kPa) 1.24 ± 0.32 13.71 ± 1.39 27.14 ± 2.40
Peak modal value (E-) (kPa) 1.10 13.18 27.24
Skewness 2.6 2.4 0.4
Em-E-Em(%) 11.3 3.9 − 0.4
Kernel size parameter (kPa) 0.05 0.63 0.88

Mean value (EmEA) ± SD (kPa)

(Elosegui-Artola et al.)

1.99 ± 0.13 13.69 ± 2.84 29.01 ± 6.18
Em-EmAEEm(%) − 37.8 0.2 − 6.4