Table 4. Effect of Different Treatment Reagents on Texture Performance.

sample specific surface area (m2/g) total pore volume (cm3/g) average pore size (nm)
WSC 116.63 0.0927 2.67
KOH 983.75 0.2653 2.11
H3PO4 736.62 0.2895 2.43
ZnCl2 209.18 0.1089 2.85
H2SO4 198.77 0.0862 3.26