Images of steel wire at different stages. (a) Immediately after immersed into solution, (b) corrosion just initiated where a rust spot was viewed, (c) corrosion in development where corrosion region has been developed, and (d) after wire breaks (The details about when and under what experimental conditions these photos were taken are given in Figure 4, respectively).