Skip to main content
. 2020 Nov 23;142(49):20814–20827. doi: 10.1021/jacs.0c10258

Figure 5.

Figure 5

Li metal intensity for the 7Li in situ NMR measurements when cycling Cu−LFP cells in LP30 with polymer-coated Cu. (a) Normalized total LiNMR intensity at the end of plating, (b) normalized dead LiNMR intensity at the end of stripping, and (c) the CE for PEO- (blue), PMMA- (yellow), and PVDF-coated (red) Cu electrodes. Measurements for bare Cu (in green) are shown here to aid comparison.