Skip to main content
. 2020 Nov 4;52(6):1117–1123. [Article in Chinese] doi: 10.19723/j.issn.1671-167X.2020.06.022

表 4.

光照强度及时间对光固化树脂水门汀氧阻聚厚度的影响

Effect of light intensity and illumination time on oxygen inhibition layer thickness of light-cured resin cement  /μm

Items 10 s 20 s 40 s 60 s F P
    n=5
800 mW/cm2 31.20±1.79 26.40±2.19 26.40±3.58 19.20±1.79 8.917 < 0.001
1 000 mW/cm2 23.20±1.79 22.40±1.79 24.80±1.79 19.20±1.79 7.704 0.002
1 200 mW/cm2 21.60±2.19 20.80±3.35 20.80±1.79 17.60±2.19 2.622 0.086
F 35.429 6.167 6.500 1.143
P < 0.001 0.014 0.012 0.351