Characteristics of the starting powders for the production of the β eutectoid bearing functionalised Ti alloys.

Powder Particle size (D90) Mesh Purity Morphology
Ti (HDH) 75 μm 200 99.4% Irregular
Cu 63 μm 230 99.7% Dendritic
Mn 45 μm 325 99.0% Angular