Skip to main content
. 2020 Sep 17;59(48):21499–21504. doi: 10.1002/anie.202009710

Figure 1.

Figure 1

a) FT‐IR spectra of (i) pristine HKUST‐1 and composites after loading at (ii) 80 °C for 6 h, then polycondensation at (iii) 90 °C, (iv) 120 °C, and (v) 150 °C for 15 h in comparison with (vi) CA; b) PXRD pattern, c) TGA plot and d) SEM images of (1) pristine HKUST‐1 and the composites prepared at (2) 90 °C, (3) 120 °C and (4) 150 °C.