Skip to main content
. 2020 Dec 21;6(7):1921–1931. doi: 10.1016/j.bioactmat.2020.12.007

Fig. 10.

Fig. 10

XRD diffractograms of MBG samples after 1 (a) and 7 (b) days of immersion in SBF. The broad peak around 23° is characteristic for Si-based glasses. Peak positions for crystalline hydoxapatite (ICDD 9–432) and calcium carbonate (ICDD 85–1108) are indicated.