Skip to main content
. 2020 Aug 24;50(6):392–405. doi: 10.5051/jpis.1905680284

Table 1. Ti6Al4V specimens used in the static state test of mechanical properties.

Cylindrical Ti6Al4V specimen with a dense core and a porous outer layer (diameter, 8 mm; height, 15 mm; solid pillar diameter, 4 mm) Cylindrical Ti6Al4V test specimen with a completely porous layer (diameter, 8 mm; height, 15 mm)
30% porosity 30% porosity
45% porosity 45% porosity
60% porosity 60% porosity