Measured water contact angle of the studied thermoplastic films (the coefficient of variation (CV) in % is in brackets below the mean values).

Thermoplastic Films Contact Angle in [deg] after the Indicated Time of Treatment in Oxygen Plasma
0 min 2 min 4 min
ABS 93 35 33
(8.3) (18.8) (15.8)
PS 85 22 0
(25.6) (17.5) (-)