TGA results of conductive PP, PLA and PP/PLA: T5%, T50%, ∆T and the remaining ash (%) at 500 °C.

Yarn Type T5% (°C) T50% (°C) ∆T (°C) Remaining Ash (%) at 500°C
PP
Modified PP
PEDOT:PSS coated PP
332
344
364
455
461
465
-
6
11
0.93
2.16
2.72
PLA
Modified PLA
PEDOT:PSS coated PLA
296
307
333
354
372
393
-
18
39
0.20
0.30
0.39
PP/PLA
Modified PP/PLA
PEDOT:PSS coated PP/PLA
315
317
336
386
412
430
-
26
44
1.16
2.46
4.84