Skip to main content
. 2020 Nov 27;10(12):2356. doi: 10.3390/nano10122356

Table 6.

Concentration (μg eq. Trolox/g sample) of 2,2-diphenyl-1-picrylhydrazyl radical (DPPH) of the active multilayer films with and without cellulose nanocrystal (CNC) coatings in the open a closed system for 15 days.

Sample Day Open System Closed System
(μg eq. Trolox/g
Sample)
(μg eq. Trolox/g
Sample)
Active monolayer 1 17.44 ± 0.14 a ---
3 15.94 ± 0.10 b,A 15.98 ± 0.19 a,A
8 14.28 ± 0.17 c,B 14.42 ± 0.02 b,B
15 12.49 ± 0.08 d,C 13.76 ± 0.12 c,D
Active multilayer with CNC 1 9.11 ± 0.09 e ---
3 7.74 ± 0.03 f,E 8.14 ± 0.02 d,F
8 7.42 ± 0.01 f,G 7.44 ± 0.01 e,G
15 6.25 ± 0.02 g,H 7.04 ± 0.12 e,I
Active multilayer without CNC 1 12.66 ± 0.12 h ---
3 10.90 ± 0.02 i,J 11.01 ± 0.06 f,J
8 9.67 ± 0.03 j,K 10.07 ± 0.03 g,L
15 9.00 ± 0.09 k,M 9.29 ± 0.04 h,M

a–k: Different superscripts within the same column indicate significant differences among samples (p < 0.05). A–M: Different superscripts within the same row indicate significant differences among samples (p < 0.05).