The composition of prepared samples: the basic mixture is composed of 12% of plasticizer and the remaining 88% is PHB/PLA in the ratio of 70/30. For filled samples, 15 wt.% of TCP is added to the mixture.

Amount (wt.%)
Sample PHB PLA Citroflex Syncroflex TCP
PHB/PLA-CT 62 26 12 0 0
PHB/PLA-CT_TCP 54 23 10 0 13
PHB/PLA-SN 62 26 0 12 0
PHB/PLA-SN_TCP 54 23 0 10 13