Skip to main content
. 2020 Dec 6;12(12):2924. doi: 10.3390/polym12122924

Figure 11.

Figure 11

SEM images of PA6 fractured surfaces at three different magnifications for the 10 (a–c) and 100 mm/min (d–f) strain rates.