Table 3.
Process | Polymer | Pore Size (µm) | References |
---|---|---|---|
Conventional gas foaming | PEGDA | 100–400 | [61,62] |
CO2-water emulsion templating | Dextran | 6.25–7 | [63] |
Dense gas CO2 + cross-linker | Elastin | 80 | [64] |
Dense gas CO2 + cross-linker | Gelatin | 80–120 | [75] |
Porogen leaching | PEG/PCL | 180–400 | [65] |
Porogen leaching | PLGA | 250–500 | [6] |
Freeze-drying | Collagen/Chitosan | 50 | [66] |
Freeze-drying | Agarose | 71–187 | [67] |
Freeze-drying | Chitosan, alginate | 60–150 | [68] |
Freeze-drying | Gelatin | 40–500 | [69] |
Freeze-drying | PVA/PCL | 30–300 | [70] |
Freeze-drying | Chitosan/PCL | 10–100 | [72] |
Electrospinning | Gelatin/PCL | 20–80 | [72,74] |