Mechanical properties of studied alloys obtained by impulse excitation.

Sample µ G (GPa) E (GPa)
TiSi2 0.28 30 ± 1 77 ± 2
TiSi2 + 20 wt.% PA 0.26 12 ± 1 30 ± 1
Ti 0.33 44 ± 1 116 ± 4
Ti + 20 wt.% PA 0.28 24 ± 1 61 ± 1
Ti + 30 wt.% PA 0.27 18 ± 1 47 ± 1
Ti + 40 wt.% PA 0.26 11 ± 1 28 ± 1