. 2020 Dec 9;13(24):5607. doi: 10.3390/ma13245607

Table 6.

The changes in weight after 7 days in SBF solution.

Sample Weight Change (g)
TiSi2 −0.023 ± 0.004
TiSi2 + 20 wt.% PA −0.050 ± 0.016
Ti 0.001 ± 0.000
Ti + 40 wt.% PA 0.003 ± 0.000