Skip to main content
. 2020 Dec 18;13(24):5783. doi: 10.3390/ma13245783

Figure 2.

Figure 2

Fiber diameter distribution in the (a) as-spun poly(ethylene terephthalate) (PET) web and (b) web after annealing at 116 °C for 5 min. The average value and coefficient of variation of the fiber diameters, as well as the SEM image of the web, are shown in the insets.