TABLE 5.
Conversion percentage for each biomass pseudo-component (between 200 and 600°C) for SG and SG with different catalysts.
| Heating rate °C/min | SG | 30KP | 30Clino | 30Bento | 10KP/10Clino | 10KP/10Bento | |
| Cellulose | 25 | 87.73 | 92.61 | 93.07 | 93.26 | 88.20 | 93.86 |
| 100 | 86.62 | 90.47 | 93.69 | 93.69 | 83.63 | 89.82 | |
| Hemicellulose + extractives | 25 | 82.01 | 65.14 | 88.46 | 91.34 | 45.06 | 69.26 |
| 100 | 81.95 | 67.80 | 88.70 | 86.58 | 44.26 | 66.93 | |
| Lignin | 25 | 67.20 | 94.34 | 89.10 | 88.68 | 88.93 | 91.52 |
| 100 | 65.51 | 90.83 | 93.64 | 93.62 | 86.96 | 93.71 |