Sorption kinetics of indigo carmine (measured in mg absorbed per gram of resin) for the chitosan matrices prepared at three different temperatures (left) and at the same temperature (170 °C) for different times (right). (Lines represent curve fittings using a pseudo second order model, Table S5).