Mean and standard deviations in MPa for the shear bond strength (SBS) among the study groups.

Surface preparation methods Ceramic type
P-value within surface preparations
VITA Suprinity® PC (n = 30)
IPS e. max (n = 30)
Group (N) N (%) of Samples de-bonded after aging Mean SBS in MPa (SD) Group (N) N (%) of Samples de-bonded after aging Mean SBS in MPa (SD)
HFA GI (10) 1 (10%) 8 b c (4.5) GIV (10) 3 (30%) 5.4 c (1.4) 0.000∗∗∗
Soflex discs GII (10) 5 (50%) 5.6 c (2) GV (10) 2 (20%) 12 a b (4)
Soflex discs & HFA GIII (10) 0 (0%) 16 a (5) GVI (10) 0 (0%) 14 a b (3.3)
P-value between ceramic types 0.04∗

N: number, SD: standard deviation, SBS: shear bond strength, MPa: mega-pascal.

∗,∗∗∗: denotes statistical significance (critical region: P < 0.05, P < 0.001).

a,b,c: denotes Post-hoc Tukey's statistical differences between the groups (critical region: P < 0.05).