a CV profile of MnO/CoMn2O4 ⊂ GN at a scan rate of 0.1 mV s−1 in the voltage range of 0.01–3.0 V. b The charge and discharge profiles of MnO/CoMn2O4 ⊂ GN. c Cycling performance and Coulombic efficiency of the CoMn2O4 and MnO/CoMn2O4 ⊂ GN electrodes at a current density of 0.1 A g−1. d Rate performances of the CoMn2O4 and MnO/CoMn2O4 ⊂ GN electrodes at various current densities. e Cycling performance of the MnO/CoMn2O4 ⊂ GN electrode at a current density of 1 A g−1