a •OH production capacity of FeO, MoS2, MoS2 + FeO, and FeO/MoS2-BSA solutions mixed with H2O2. b, c Temperature curves of different concentration FeO/MoS2-BSA under irradiation with 1064 nm and 808 nm laser (1 and 0.3 W cm−2 separately). d PT-enhanced •OH generation of FeO/MoS2-BSA nanocomposites with or without 1064 nm laser irradiation (0.75 W cm−2)