Fig. 11.
a Schematic illustration of multilayered Ti3C2Tx particle containing shallow and deep adsorption sites near the gap opening and in its interior, respectively, b Capacitance of Ti3C2Tx/carbon black–PTFE laminate in a Swagelok cell measured at scan rates of 2 and 20 mV s−1 (dash line and symbols, respectively) in 1 M MgCl2 related to deep and shallow adsorption sites, respectively.
Reprinted with permission from Ref. [66]. Copyright © (2015) John Wiley & Sons, Inc. c Electroadsorption and regeneration cycles of porous Ti3C2Tx electrode in 500 mg L−1 NaCl solution. d Electroadsorption capacitance of porous Ti3C2Tx at varied voltage in 500 mg L−1 NaCl solution. Reprinted with permission from Ref. [62]. Copyright © (2018) Elsevier Inc. e Schematics of the CDI process. Reprinted with permission from Ref. [60]. Copyright © (2018) Elsevier B.V