Skip to main content
. 2019 Dec 30;12:13. doi: 10.1007/s40820-019-0346-1

Fig. 7.

Fig. 7

a Relative density obtained at different sintering temperatures with WC composites with 6 wt% ZrO2 (stabilized with varying amount of Y2O3) sinter-additive [111]. Densification curves for b pure WC sintered at 1800 °C for holding 5 min, c WC3Z and WC10Z specimens sintered at 1600 °C for holding 5 min [104].

Figure panels reproduced from Ref. [111] with permission from Elsevier copyright 2005, Ref. [104] with permission from Elsevier copyright 2013