Skip to main content
. 2019 Dec 30;12:13. doi: 10.1007/s40820-019-0346-1

Table 3.

Average grain size and relative density of pure WC and WC–Al2O3 composite after the same HFIHS sintering conditions with same staring WC powders [102]

Composition Relative density (%) Grain size (nm)
WC 97 265
WC–5 vol% Al2O3 98 185
WC–10 vol% Al2O3 99 138
WC–15 vol% Al2O3 99.8 101