Skip to main content
. 2021 Jan 4;19(2):1737–1763. doi: 10.1007/s10311-020-01147-x

Table 4.

Characteristics of non-woven mats made out of silkworm silk dope. Spider silk mats

Characteristic Bombyx mori References
Fiber diameter (nm) 6.5 to 6100 Zarkoob et al. (2003); Min et al. (2004); Ayutsede et al. (2005); Meinel et al. (2009); Aznar-Cervantes et al. (2012); Zhang et al. (2012)
Morphology

Beads to cylindrical (low dope concentration)

Continuous to ribbon-like (high concentration)

Min et al. (2004); Zhang et al. (2012)
Ultimate tensile strength (MPa) 13.5 to 74 Jin et al. (2004); Amiraliyan et al. (2010); Yi et al. (2018); Mohammadzadehmoghadam and Dong (2019)
Strain at break (%) From 4 to 40 Ohgo et al. (2003); Jin et al. (2004); Amiraliyan et al. (2010); Zhang et al. (2012); Mohammadzadehmoghadam and Dong (2019)
Porosity (%) 62 to 68 Min et al. (2004); Mohammadzadehmoghadam and Dong (2019)
Water uptake capacity (%) 405 Mohammadzadehmoghadam and Dong (2019)
Temperature of degradation (°C) 250 Pang et al. (2019)