. 2020 Dec 11;11(1):43–59. doi: 10.1021/acscatal.0c04290

Figure 8.

Figure 8

Crystallite size of Ni/NiCu metal formed during DRM at 800 °C as a function of time obtained by Rietveld refinement of the in situ collected XRD patterns of La2Ni0.8Cu0.2O4 and La1.8Ba0.2Ni0.9Cu0.1O4 samples.