Table 3.
Experimental plan of the tensile tests.
Material State | T6 | SS |
---|---|---|
DC density (A/mm2) | 0, 5, 10, 20, 30 | 0, 5, 10, 20, 30 |
Rolling direction (deg) | 0 | 0 |
Strain rate (s−1) | 0.1 | 0.1 |
Repeatability | 3 | 3 |
Experimental plan of the tensile tests.
Material State | T6 | SS |
---|---|---|
DC density (A/mm2) | 0, 5, 10, 20, 30 | 0, 5, 10, 20, 30 |
Rolling direction (deg) | 0 | 0 |
Strain rate (s−1) | 0.1 | 0.1 |
Repeatability | 3 | 3 |