Swelling behavior of synthesized P(NIPAAm-co-DMAEMA) hydrogel in different conditions

Temperature (°C) pH ESR
25 6.5 3.1 ± 0.36
37 7.4 0.2 ± 0.022
37 5.8 0.225 ± 0.025
40 7.4 0.025 ± 0.019
40 5.8 0.46 ± 0.13

The data were reported as the mean ± standard deviation of three independent measurements