Skip to main content
. 2020 Jun 8;2:100029. doi: 10.1016/j.bioflm.2020.100029

Table 1.

Nanoparticle characterisation. Size determined by TEM and DLS, and surface charge measured by Zeta potential.

Sample Size by TEM (nm) Size by DLS (nm) PDI Zeta potential (mV)
Bare Image 1 54.0 (±6.9) 79.7 (±0.7) 0.025 (±0.02) −37.3 (±2.4)
Amine Image 2 57.3 (±4.3) 105.5 (±4.4) 0.169 (±0.04) +29.3 (±0.4)
Epoxy Image 3 58.7 (±5.9) 83.6 (±3.7) 0.071 (±0.03) −27.7 (±0.6)
Hydroxy Image 4 57.8 (±7.4) 85.1 (±3.7) 0.073 (±0.03) −38.9 (±3.3)