. 2020 Dec 24;143(1):279–285. doi: 10.1021/jacs.0c10397

Figure 2.

Figure 2

DEMS data of an experiment in which the electrolyte of 0.5 M NaClO4 containing 1 mM HClO4 was purged with Ar. (A) CV; (B) ionic current for mass 2. Sweep rate: 20 mV/s. Flow rate: 5 μL/s. Working electrode: polycrystalline gold.