Table 2.

Flexural strengths (MPa) of the coated and uncoated specimens of high powder-liquid and resin-modified glass ionomer cements.

Flexural strengths (MPa) Uncoated Coated
Equia Forte Fil 15.32 ± 1.15a 41.47 ± 0.89b
Fuji II LC 52.90 ± 2.17c 104.77 ± 3.97d

The superscripts with different small letters indicate a significant difference in flexural strength between the groups.