Skip to main content
. 2021 Jan 4;11(1):96. doi: 10.3390/nano11010096

Figure 5.

Figure 5

Figure 5

Figure 5

Figure 5

(A) Degradation of 100 µm PVA/silver films heated at 80 °C for 90 m and then immersed in water; (B) degradation of 200 µm PVA/silver films heated at 80 °C for 90 m and then immersed in water; (C) degradation of 100 µm PVA films heated at 110 °C for 90 m and then immersed in water; (D) degradation of 200 µm PVA/silver films heated at 110 °C for 90 m and then immersed in water; (E) degradation of 100 µm PVA films heated at 140 °C for 90 m and then immersed in water; (F) degradation of 200 µm PVA films heated at 140 °C for 90 m and then immersed in water.