GL13K-TAMRA peptide loading and release from peptide-coated collagen scaffolds. (A) CLSM micrographs of pristine non-mineralized and mineralized collagen samples with and without GL13K-TAMRA coating. All scale bars are 100 μm. Inserts are digital photographs of the hydrogels in waters. (B) Quantification of GL13K-TAMRA loaded on non-mineralized and mineralized collagen scaffolds. (C) Cumulative GL13K-TAMRA release for up to 28 days from non-mineralized and mineralized collagen scaffolds.