Cesium distribution on PB/cellulose aerogel after adsorption. (A) SEM image of the cryo-fractured PB composite. (B) EDS mapping of iron. (C) EDS mapping of cesium. (D) EDS mapping of iron–cesium overlay. Reproduced with permission from [39].