Skip to main content
. 2021 Jan 15;13(2):274. doi: 10.3390/polym13020274

Figure 14.

Figure 14

SEM images of tensile fractured surface of the (a) TPS film (b) TPS-3wt%DOL (P) (c) TPS-3wt%DOL (U) (d) TPS-5wt% DOL (P) and (e) TPS-5wt%DOL (U) biocomposite films at 500× magnification (left) and 1000× magnification (right).