Table 3. Sampling Details for the Deposition of ZnO Thin Films with IPA at Different Temperaturesa.
| glass
substrate thickness (nm) |
copper
foil substrate thickness (nm) |
|||
|---|---|---|---|---|
| deposition temperature (°C) | sonication | without sonication | sonication | without sonication |
| 30 (20 cycle) | G1(136 ± 34) | G4(380 ± 19) | C1(364 ± 11) | C4(438 ± 10) |
| 50 (20 cycle) | G2(660 ± 12) | G5(864 ± 22) | C2(283 ± 10) | C5(848 ± 11) |
| 50 (30 cycle) | 3330 ± 87 | 2660 ± 64 | ||
| 50 (40 cycle) | 8780 ± 219 | 7870 ± 228 | ||
| 65 (20 cycle) | G3(470 ± 10) | G6(960 ± 18) | C3(318 ± 11) | C6(955 ± 95) |
Thickness and number of dipping cycle associated with the deposited films are shown in the parentheses.