Skip to main content
. 2021 Jan 27;13(3):399. doi: 10.3390/polym13030399

Figure 13.

Figure 13

Calorimetric analyses were performed on the specimens obtained by FDM with different Tb. (a) Tn = 200 °C; (b) Tn = 230 °C.