Skip to main content
. 2021 Jan 28;13(3):413. doi: 10.3390/polym13030413

Table 4.

Ensile strength properties in the machine direction of the recycled PP/LLDPE/PP-24L multilayer films following different recycling processes.

Recycled Samples Tensile Strength at Yield (MPa) Tensile Strength at Break (MPa) Elongation at Break (%)
Monolayer film
R1-PP/LLDPE/PP-24L 6.3 ± 1.3 15.5 ± 3.5 213.7 ± 20.0
Tensile test rectangular specimen
R2-PP/LLDPE/PP-24L 10.0 ± 0.5 20.3 ± 0.2 140.5 ± 14.2
R3-PP/LLDPE/PP-24L 10.8 ± 0.3 18.1 ± 0.1 120.3 ± 11.0