Skip to main content
. 2021 Jan 21;14(3):517. doi: 10.3390/ma14030517

Figure 4.

Figure 4

Figure 4

Compressive strength of epoxy latexes modified mortar under three curing regimes: (a) 0%, (b) 5%, (c) 10%, (d) 15%, and (e) 20%.