Table 1.

Surface energy components and water contact angles (WCAs) of glass and PGS samples cured at different temperatures, calculated from contact angle data, and using the OWRK equation.

Material σd (mN/m) σp (mN/m) σtotal (mN/m) WCA (°) σptotal
Glass 16.43 34.03 50.47 45.30 ± 4.82 0.67
130 °C 14.48 18.48 32.96 71.16 ± 1.43 0.56
150 °C 17.72 18.08 35.8 68.07 ± 3.94 0.51
170 °C 15.5 19.84 35.34 67.46 ± 3.94 0.56